A novel and greener sequential column leaching approach for the treatment of two different Greek laterites

Komnitsas Konstantinos, Petrakis Evaggelos, Bartzas Georgios

Απλή Εγγραφή


URIhttp://purl.tuc.gr/dl/dias/440A0D54-3824-41D9-A657-D0FB9D9D3BFC-
Αναγνωριστικόhttps://doi.org/10.1016/j.scitotenv.2022.158748-
Αναγνωριστικόhttps://www.sciencedirect.com/science/article/pii/S0048969722058478-
Γλώσσαen-
Μέγεθος9 pagesen
ΤίτλοςA novel and greener sequential column leaching approach for the treatment of two different Greek lateritesen
ΔημιουργόςKomnitsas Konstantinosen
ΔημιουργόςΚομνιτσας Κωνσταντινοςel
ΔημιουργόςPetrakis Evaggelosen
ΔημιουργόςΠετρακης Ευαγγελοςel
ΔημιουργόςBartzas Georgiosen
ΕκδότηςElsevieren
ΠερίληψηΤhe present study investigates, from an environmental protection viewpoint, the efficiency of sequential column leaching of two different Greek laterites, i.e. a limonitic ore from central and a saprolitic ore from northern Greece. First, the most refractory limonitic laterite is leached in the first column for 15 days and the obtained pregnant leach solution (PLS) is further used for the leaching of the easier to treat saprolitic ore in the second column, thus achieving a significantly reduced acid consumption. The main parameters affecting the process efficiency, i.e. acid molarity (1.5 or 3 mol/L H2SO4) and addition of sodium sulfite (Na2SO3) in the leaching solution were studied. The extraction of Ni, Co, Fe, Al, Mg, Mn and Ca was determined by Atomic Absorption Spectroscopy (AAS), while the characterization of the ores and final residues was carried out by X-ray fluorescence (XRF), X-ray diffraction (XRD), Fourier-transform infrared (FTIR) spectroscopy, thermogravimetric analysis (TGA/DTA), and Scanning Electron Microscopy/Energy Dispersive X-Ray Spectroscopy (SEM-EDS) analysis. The results confirm the efficiency of the proposed green approach, which with the use of leaching solution containing 1.5 mol/L H2SO4 and 20 g/L Na2SO3 resulted in 73.8 % Ni, 71.6 % Co and 8.4 % Fe extraction after a short period of time (33 days), while the acid consumption, which is a serious environmental concern, was very low and did not exceed 300 kg/t ore. Overall, the proposed process not only improves the efficiency of leaching of different types of laterites for the recovery of both Ni and Co but also reduces the environmental impacts due to the significantly lower acid consumption.en
ΤύποςPeer-Reviewed Journal Publicationen
ΤύποςΔημοσίευση σε Περιοδικό με Κριτέςel
Άδεια Χρήσηςhttp://creativecommons.org/licenses/by/4.0/en
Ημερομηνία2024-01-04-
Ημερομηνία Δημοσίευσης2023-
Θεματική ΚατηγορίαLimonitic/saprolitic lateritesen
Θεματική ΚατηγορίαSequential column leachingen
Θεματική ΚατηγορίαSulphuric aciden