Institutional Repository
Technical University of Crete
EN  |  EL

Search

Browse

My Space

Correlation of surface characteristics with catalytic performance of potassium promoted Pd/Al2O3 Catalysts: The case of N2O reduction by alkanes or alkenes

Pekridis Georgios, Kaklidis Nikolaos, Konsolakis Michail, Iliopoulou Eleni, Yentekakis Ioannis V., Marnellos George E.

Simple record


URIhttp://purl.tuc.gr/dl/dias/33E1F576-26B7-4262-BCEB-BDE2F7DA123F-
Identifierhttps://doi.org/10.1007/s11244-011-9735-5-
Languageen-
Extent7en
TitleCorrelation of surface characteristics with catalytic performance of potassium promoted Pd/Al2O3 Catalysts: The case of N2O reduction by alkanes or alkenesen
CreatorPekridis Georgiosen
CreatorΠεκριδης Γεωργιοςel
Creator Kaklidis Nikolaosen
CreatorKonsolakis Michailen
CreatorΚονσολακης Μιχαηλel
Creator Iliopoulou Elenien
Creator Yentekakis Ioannis V.en
Creator Marnellos George E.en
PublisherSpringer USen
DescriptionΔημοσίευση σε επιστημονικό περιοδικό el
Content SummaryThe present study aims at investigating the role of potassium (K) promoter on the surface and catalytic behavior of Pd/Al2O3 catalysts during N2O reduction by alkanes (CH4, C3H8) or alkenes (C3H6). In this context, the surface properties of un-promoted and K-promoted catalysts were evaluated by means of X ray photoelectron spectroscopy (XPS), in situ diffuse reflectance infrared Fourier transform spectroscopy (DRIFTS) of CO adsorption and FTIR-pyridine adsorption. The results reveal that both the electronic and structural properties of Pd entities can be substantially modified by potassium ions, which are in close proximity with catalyst surface without exhibiting a tendency to accumulate. This in turn results in significant modifications on reactants/intermediates chemisorption bonds, affecting the catalytic performance of K-promoted catalysts. Indeed, it was found that potassium strongly promotes the N2O reduction by propane or propene yielding notably lower N2O light off temperatures (ca. 100 °C) as compared to those obtained over un-promoted catalysts. On the contrary, a slight inhibition upon K-promotion was observed, when using CH4 as reducing agent, implying that the action of the K-promoter is strongly related with the reducing agent used and its’ relative interaction with the catalyst’s surface. The results are discussed in terms of the correlation between the surface chemistry modifications induced by electropositive promoters and the de-N2O performance of K-promoted catalysts.en
Type of ItemPeer-Reviewed Journal Publicationen
Type of ItemΔημοσίευση σε Περιοδικό με Κριτέςel
Licensehttp://creativecommons.org/licenses/by/4.0/en
Date of Item2015-11-04-
Date of Publication2011-
SubjectPalladium en
SubjectPotassium promoteren
SubjectFTIR-pyridine adsorptionen
Bibliographic CitationG. Pekridis, N. Kaklidis, M. Konsolakis, E. Iliopoulou, I.V. Yentekakis, G.E. Marnellos, "Correlation of surface characteristics with catalytic performance of potassium promoted Pd/Al2O3 catalysts: The case of N2O reduction by alkanes or alkenes" Top. in Catal., vol. 54, no. 16-18, pp. 1135-1142, Aug. 2011. doi:10.1007/s11244-011-9735-5en

Services

Statistics